Unacceptable Conditions

Oxidized spots, weak heated and burnt sheet are not acceptable

Acceptable Conditions

Slight traces of rust and dry mould on the packaging and interior sheets are acceptable but it should not be >30% of the bales sampled. Large particles, bubbles or barks, small stains or blisters, slightly sticky, slightly under-cured or over-smoked rubber, blemishes are permissible.