Skim Rubber

The skin fraction that is a by- product of centrifuging process, has 3% – 4% rubber content. Such a low percentage plus an increased proportion of non-rubber constituents demand that to recover the rubber, a very strong acid be used. Such a recovery using sulphuric acid has its ill effects on the rubber content. This grade, though not technically good, is still very viable economically and is used in non-critical applications.