RSS 1X

Unacceptable Conditions

Oxidized spots, weak heated, under-cured, over-smoked, opaque and burnt sheet are not acceptable.

Acceptable Conditions:

Slight traces of dry mould on the packaging are acceptable but mould should not penetrate inside the bale. Small scattered pinhead bubbles are permissible.